Aluminum Fibered Rubberized Roof Coating Français
Description
This rubberized and fibered aluminum coating CR-390 is formulated with asphalt, selected resins, fibers and a large quantity of aluminum powder. That excellent coating confers excellent characteristics such as flexibility, weather resistance and sun reflection. This product gives, once dry, a reflective, glossy and durable finish that protects against UV and oxidation. For roofs, flashings, utility buildings and metal structures this fibered paint is also perfect to patch and fill tinny cracks and screw heads. We recommend CR-390 in combination with Condor Flex line products.
Surface Preparation
Avoid application if showers are foreseen. Surfaces must be sound, clean and free of dust, dirt, rust, oil, grease, chipped paint, frost or any other contaminants. Previously­ fill holes, cracks and weak spots with CONDOR Rubberized plastic cement CR320.
Application
Stir product well before use. Apply with a squeegee, a brush, a roller or a paintbrush. Avoid over-brushing. First, apply a coat on overlaps and nails; than, apply a coat uniformly over all the surface. To ease application in cold season, keep product in a warm place.
Cleanning
Clean tools and equipment with mineral spirits.
Norm
CAN/O.N.G.C. 37.42-M89 type II
Package
Available on 3,78L and 18,9L format.
Shelf Life
12 months after purchasing date when kept in its tightly closed original container.
Technical Data Table
Specifications  
Color Aluminum
Solids by Volume 60 to 70 %
Weight 1,0 kg/L (8,3 pounds/gal)
Coverage 1,0 to 2,25 L/m² (2 to 4,5 gal/100 ft²)
Dry Time*

To 50 % R.H. 20°C (68°F)

To the Touch* 4 to 8 hours
Completely Dry* 48  to 72 hours
Service Temperature -30°C à 80°C (-22°F to 176°F)
Application Temperature Can be applied at low temperature but preferably above 10°C (50°F).
Chemical Resistance

Resistant to water calcium chloride, salt and to lightly acid or alkaline solutions. Do not resist to oils, greases and solvents.

Permeance to Water Vapor (ASTM E96) 3 mm (1/8'') coat before drying 2.9 ng/Pa.m2.s (0.05 perms)
 

* Drying Time depend of surface porosity and temperature.

Restriction
Avoid contact with polystyrene insulation foam or any solvent alterable materials. If product is applied near a ventilation unit or an air conditioner, take necessary precautions to avoid infiltration solvent odor inside. It is not recommended on bare wood or on porous surfaces. Make sure that bituminous surfaces or coal tar coatings are stable, completely dry and free of volatile residues. This product may change color in aluminum oxidizing environments. Do not apply if showers are foreseen or if there is a possibility of dew point before it is completely dry. Humidity can tarnish freshly applied coating. Do not apply on wet surfaces. Protect freshly applied product and open container from open flame and adjacent welding activity. For EXTERIOR USE ONLY.
Warranty
The customer shall verify of the suitability of this product for the intended purpose. Applicator's skill, weather and surface conditions being beyond manufacturer's control, we limit our liability to replacement of defective material only in sealed container, within 1 year of proof of purchase. FOB plant.

Aluminum Fibered Rubberized Roof Coating
Aluminum Fibered Rubberized Roof Coating
Sans Amiante
Avertissement Simdut Simdut

CONTENTS MAY CATCH FIRE: Contains petroleum distillates. May cause dizziness, headache or nausea. May cause nose, throat, eyes and skin irritation. Keep away from heat sources, sparks and flames. Do not smoke. Use only with adequate ventilation. Do not breathe vapors. Wear safety glasses and appropriate gloves. KEEP OUT OF REACH OF CHILDREN.


FIRST AID TREATEMENT: Eyes : In case of contact, flush immediately with plenty of water for at least 15 minutes and get medical attention immediately; for skin, wash thoroughly with soap and water. If you experience difficulties in breathing, leave the area to obtain fresh air. If difficulties continues, get medical assistance immediately. If swallowed, do not induce vomiting. Get medical attention immediately.
 
PDFdownload PDF version